old-timer tin and copper lures

tintin1

New member
Help!

I'm looking to put a brass or copper back to some tin lures and I have not been able to find suitably thin sheets of the metals. 

Either that or I have not been able to find a way to press the metal properly into the mould before casting the tin or white metal. 

So - where do I start to look for thin shim metal? What trades still use it?  Hobby shops near me are hopeless.

And if anyone who has done this before has hints as to how to manage a thicker sheet (0.5mm copper is as thin as I can find in an art-supply shop) I'd be glad of the help.  

The reason I want to do this is that a mate standing next to me was throwing a v-back copper and tin spoon and got noticeably more hits than I was getting on a v-back tin spoon.  Not for the first time either.  The soft, almost buttery shine that the copper gives off can look a lot better than the harder glitter I get from the 100% tin spoon. 
 
It is called a two tone,these spoons have been used for ages and is still very DEADLY.
The way it is done is that they Heat weld(fusion) the two metals together ,there is not allot of guys that do this ,but I reckon if you go to any sheet metal shop in your area they should be able to help.

I have used these spoons and still have a couple. The idea is that you do not want the copper to shine too much it must not be dull.  But some where in between.

shad,garrick,cob and even rockcod love them.

 
 
Interesting!
I have not tried it but I have thought about it... Maybe try applying some soldering flux to the copper first. The flux comes in a past, rub it on first, then pour the lead. Let us know how it goes..

Cheers
Bennie
 

PH

Senior Member
tintin1 wrote:
Help!

I'm looking to put a brass or copper back to some tin lures and I have not been able to find suitably thin sheets of the metals. 

Do you have a branch of (the world-wide) Non Ferrous Metals in Perth?

Here in SA they sell off-cuts of any material - even paper thin copper and brass shim and foil, 150mm wide

Good luck
 

tackle whore

Senior Member
you get a foil in copper same as the foil in the foiling thread i posted . if you want can send you some am sending jigs to Denis B in AUST soon .
 

tintin1

New member
thanks for the offer - i may take that up soon; right after have tried to press   some shim copper that I found after striking out with the Non Ferrous Metals hint that P H suggesed.  A computer repair store uses it and sold me some.

It is 0.152mm and looks as though it will go well into a mould.  I'll be trying it next weekend and will let you know how I go.
 

tintin1

New member
Got all the bits now and been playing.  Not too successfully yet.  I suspect pouring temperature and the mould temp is going to have to be just right.  Also a very thin film of flux.  I get the feeling that I am one trick away from getting it right.

As any plumber will tell you, you cannot get white metal to stick to copper properly without flux.  The trouble is that the flux I have found sends to splutter and hiss when hot metal gets onto it.  Lots of gas given off, which tends to blow the metal out of the mould as I am filling it.   

For all the practical blokes out there with some training in the use of solders and fluxes can you suggest something I can use that will not splutter and hiss when the hot metal gets onto it?  Or is there a way to treat the copper so that I do not need the flux?

 

 
 
tintin1 wrote:
Got all the bits now and been playing.  Not too successfully yet.  I suspect pouring temperature and the mould temp is going to have to be just right.  Also a very thin film of flux.  I get the feeling that I am one trick away from getting it right.

As any plumber will tell you, you cannot get white metal to stick to copper properly without flux.  The trouble is that the flux I have found sends to splutter and hiss when hot metal gets onto it.  Lots of gas given off, which tends to blow the metal out of the mould as I am filling it.   

For all the practical blokes out there with some training in the use of solders and fluxes can you suggest something I can use that will not splutter and hiss when the hot metal gets onto it?  Or is there a way to treat the copper so that I do not need the flux?

 

 
What you can try is to put the flux on the copper, then burn it before placing it in the mould.

Another idea, first put some flux on the copper. Then solder onto the back. As long as there is lead solder on the back it should marry with the lead you are pouring.

Keep us posted!
 

Foxhat

Senior Member
You gonna laugh but I gave up putting the copper or brass shim stock in the mold for pouring 25 years ago!

Now I glue the shimstock onto the spoon with genkem or pattex.

Step1: Prepare both surfaces to be glued by sanding
Step2: apply adhesive to both surfaces and allow to dry about 20min
Step3; Bond the 2 surfaces accurately
Step4: Put the spoon back into the mold and clamp the mold in a bench vice overnight.
Step5: Clean up with a file and drill the holes from the shimstock side.

Don't knock it till you've tried it, my Dad taught me this many years back. I've got glued spoons that I've used for the last 20 years still in my tackle bag!
 

tintin1

New member
I never laugh at advice based on experience...  Clamping in a mould will make for good and tight contact because the pressure would be taken by the shim/lure interfaces and nowhere else.

And heating the fluxed piece before pouring may get rid of the gas issue.

I'll try both ways (BJ and FH) and see what is easier and /or more satisfying.  Let u know.

 

 
 

tintin1

New member
just about there now.   I got these out of the mould thanks to that tip about heating the flux.  You need to coat the one surface, heat the coating and pour off the drop or two of residue.  Prepared that way, you can pour the tin onto the copper anytime - does not have to be hot.

 

these spoons are about 60g, have had a flat surface incorporated in the shoulder area that grabs the water well and gives the spoon a rolling flicking action.  The roll appears slow, the flick appears quick.  I have no doubt that as soon as I find some fish this spoon will tempt them better than most. 

 

So now I have to get faster at it and neater...... 
 

Attachments

  • P1010060.JPG
    P1010060.JPG
    52.4 KB · Views: 280

PH

Senior Member
I'm glad you got it right! I electroplated copper to polyurethane castings this afternoon. The results were not really satisfactory.  Plating lead with copper did not work  either. Your process seems to be the answer as far as lead is concerned
 
Top